Industeel SIRIUS 800 Heat Resistant Alloy
Subcategory: Superalloy; Iron Base
Key Words: EURONORM X8 Ni Cr Al Ti 32.21 - 1.4959, AFNOR Z10 NC 21.31, WERKSTOFF Nr 1.4876, BS NA 15(H), UNS N08800, N08810, N08811
Material Notes: Description: The SIRIUS® 800, H and H+ grades are three variants of a high chromium and nickel austenitic alloy which combines good corrosion and creep resistance. SIRIUS® 800 is employed at temperature below 600°C(1112°F) while SIRIUS® 800H and SIRIUS® 800H+ are used above 600°C (1112°F). CLI heats obtained by vacuum degasing process have a tight control of the chemical analysis including residual elements in order to improve the weldability and in-service properties.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Annealing Point
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|