Industeel NUCL 18.10 B4 Natural Boron (Min 1% wt) Alloyed 304 Stainless Steel
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: aisi304, aisi 304, DIN W.14306 Bor-01 Ind.00, ASTM A887 UNS S30464 : Type 304B4, SUS304, SS304
Material Notes: Description: Isotope B10 has the property to capture neutrons produced by nuclear reactions. Natural boron contains about 19.9 at% or 18.45 wt % of B10 isotope, the remaining being B11 isotope. NUCL 18.10 B4 grade is a 304 stainless steel obtained by ingot casting and alloyed with 1 to 1,24 wt% natural boron additions. In order to avoid ferrite grain which reduce the ductility of the alloy, NUCL 18.10 B4 grade has been overalloyed in Nickel when compared to 304 grades. Molybdenum additions are sometimes considered to increase the corrosion resistance properties. The ingots rolled into plates are considered for nuclear applications (transport, casks, storage -in pools) of nuclear (waste) products. For specific purposes, some other grades are sometimes used. The boron content may thus be included in the 0.2-2 weight % range or/and alloys obtained by powder metallurgy (A type). CLI-FAFER can also produce 18-10 A or B type boron alloyed grades (included B10 enriched grades). Among the family of boron enriched 304 grades, NUCL 18-10 B4 grade is the most commonly used.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|