Industeel URANUS® 65 310 L Modified Grade - C < 0.020, Si < 0.3 for Nitric Acid Services

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal; Austenitic

Key Words: EURONORM X1 Cr Ni 25.21 - 1.4335, AFNOR Z1 CN 25.20, WERKSTOFF Nr 1.4335, ASTM 310 L NAG

Material Notes:
Description: URANUS® 65 is a 25 Cr 20 Ni austenitic stainless steel with sharp control of the residual elements in order to provide high corrosion resistance properties in boiling 50-65% Nitric acid solutions. The silicon content is kept under 0.3% while the carbon content is lower than 0.015%. Molybdenum additions are also well known to reduce the behavior of the steel in nitric acid solutions. This explains why the molybdenum content is guaranteed lower than 0.3%. The sharp control of Carbon, Silicon and phosphorus contents makes it possible to produce a more stable austenite microstructure, free of intermetallic or carbide precipitations. The alloy is designed for nitric acid applications. The grade is not recommended for concentrated nitric acid purposes or highly oxidizing nitric acid solutions (with Gr VI species...)

Iron content calculated as remainder.

Information provided by manufacturer.

Available Properties
  • Density
  • Hardness, Brinell
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Yield
  • Modulus of Elasticity
  • Poissons Ratio
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。