Industeel URANUS® B26 6 Mo High Performance Super-Austenitic Stainless Steel with PREN = 43
Subcategory: Stainless Steel; Metal; Austenitic
Key Words: EURONORM X1 Ni Cr Mo Cu N 25.20.7, AFNOR Z2 NCDU 25.20.06 AZ, DIN W.Nr 1.4529 ; VD TÜV Blatt 502, UNS N08926
Material Notes: Description: URANUS® B26 (UR B26) is a 25% Ni, 20% Cr, 6% Mo superaustenitic stainless steel grade with 0.2 % nitrogen additions, particularly designed for high structural stability and high corrosion resistance properties. The 25% nickel and 1% copper additions combined with the chromium and molybdenum additions improve the behavior of the steel in many corrosive solutions encountered for example in chemical and petrochemical processes. The alloy behaves particularly well in sulphuric acid solutions and is well adapted for pollution control equipments (scrubbers...) The alloy is also seawater resistant and has extensively been used in offshore industries. The fully austenitic microstructure produced by the 25% nickel addition explains its high toughness at temperatures as low as -200°C (-328°F).
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Vickers
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Poissons Ratio
- Charpy Impact, Notched Low Temp
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|