Industeel SUPERELSO® 960 HLE Steel for Welded and Weight-Saving Structures
Subcategory: Carbon Steel; Medium Carbon Steel; Metal
Key Words: EE 960 TIIK4 according to NFA 36-204, S 960 QL according to EN 10137-2
Material Notes: Description: SUPERELSO® 960 is quenched and tempered steel for structure with higher strength. Thanks to a minimum yield strength of 960 N/mm² (140 KSI), SUPERELSO® 960 enables to make weight savings or support higher stresses and thus carry higher payload. With a good quality of steel making process, an adapted chemical analysis (low alloying content) and an excellent precision in Industeel's fabrication process (thickness tolerance, uniform mechanical characteristics), SUPERELSO® 960 is easy to machine, to bend and to weld which simplify production and maintenance. By using S SUPERELSO® 960 and thus thinner plate in welded structures, you limit preheating conditions, you decrease quantity of consumables, welding time and so production costs.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Charpy Impact, Notched Low Temp
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|