Industeel CLC 1.2311 Prehardened Mold Steel (300HB/30HRC)
Subcategory: Carbon Steel; High Carbon Steel; Mold Steel; Metal
Key Words: AFNOR 40CMD8, DIN 40CrMnMo7, WERKSTOFF.Nbr 1.2311, AISI P20
Material Notes: Description: CLC 1.2311 is a 300HB (30HRC) pre-hardened grade specially designed for plastic mold industry. Chromium, Molybdenum, carbon and manganese additions are optimized to have a fully martensite-bainite microstructure after quenching. The steel is melted in electrical furnace and refined with VOD or DH device The cleanliness of the steel is guaranteed as well as the soundness. This makes the steel particularly well adapted for mold steel even when polishing or chemical etching are required for surface finish quality.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact
- Charpy Impact, Notched Low Temp
- Charpy Impact, Unnotched
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|