Industeel CLC 1.2316S Prehardened Mold Steel (300HB) with Improved Machinability
Subcategory: Carbon Steel; High Carbon Steel; Mold Steel; Metal
Key Words: AFNOR Z40CD16 (S), DIN X36CrMo17 (S) - X33CrS16, WERKSTOFF Nbr 1.2316 with S addition - (» 1.2085)
Material Notes: Description: CLC 1.2316 S grade is a 16%Cr 1%Mo mold steel with improved corrosion resistance properties, thanks to the chromium and molybdenum additions. Furthermore specific sulfur additions are considered to increase the machinability properties. The grade in the quenched tempered condition has a fully bainite martensite microstructure and can be delivered in the prehardened condition (300HB or 340HB). The grade is not designed for highly finish polished surfaces or etched surfaces. The grade is commonly used for mold steel applications including cores, inserts, molds… subjected to wet working conditions and / or storage conditions. The grade is also used for the manufacturing of corrosive materials like PVC.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|