Industeel TENASTEEL® Cold Work Tool Steel
Subcategory: Tool Steel; Carbon Steel; High Carbon Steel; Metal
Material Notes: Description: TENASTEEL is a cold work tool steel, combining a high wear resistance together with a very high toughness. Its other advantages are a good machinability in the as-delivery condition and a particularly high resistance to thermal softening. The steel is delivered in the soft annealed condition with a maximum hardness of 250 HB. TENASTEEL is specially designed to replace D2 type steels widely used by toolmakers but suffering from an excessive brittleness. Thanks to its chemistry increasing resistance to softening during tempering, TENASTEEL is especially suited for all processes of surface treatment and coatings commonly used in the market, including nitriding processes involving high temperatures.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell C
- Modulus of Elasticity
- Compressive Strength
- Charpy Impact, Unnotched
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|