Industeel CREUSABRO® 4800 Advanced Technology in Wear Steel
Subcategory: Carbon Steel; Medium Carbon Steel; Metal
Material Notes: Description: CREUSABRO® 4800(P) is a wear resistant steel offering up to 50% extra in service life compared with a 400 HB water quenched steel. CREUSABRO® 4800(P) combines several modern metallurgical concepts which, depending on thickness, use different combinations of an enriched chemical analysis (Cr, Mo, Ti…) and controlled quenching rate. Creusabro® 4800(P) is designed to provide the optimum combination of wear resistance controlled hardness and ease of processing. Rather then using just a high hardness level, it achieves this aim by using proven and controlled metallurgical mechanisms, which are more complex but more efficient then the simple effect of hardness alone.- Work-hardening and Cr Mo micro-carbides, the basic CREUSABRO® concept
- TRIP(TRansformation Induced by Plasticity) effect originally developed with CREUSABRO® 8000
- Reinforcement of the structure with Titanium carbides.
The limited as delivered hardness of Creusabro® 4800(P) makes processing operations like cutting, machining and forming no more difficult then processing 400HB water quenched steel. Creusabro® 4800(P) is ideal for applications in mines and quarries, cement and the Steelmaking industries, publics works and agricultural machinery. It is suitable for all types of abrasion, sliding or impact, dry or wet media including high temperature abrasion up to 350°C.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact, Notched Low Temp
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|