Industeel CREUSABRO® 8000 High Performance Wear Resistant Steel
Subcategory: Carbon Steel; Medium Carbon Steel; Metal
Material Notes: Description: CREUSABRO® 8000 is a high performance wear resistant steel, exhibiting a wear resistance of 50% higher than that of conventional 500 HB water quenched steel. CREUSABRO® 8000 is using an innovative concept, based on a unique combination of chemical analysis and heat treatment procedures (oil quenching). This confers to the steel an improved wear resistant by the contribution of:- a very fine distribution of chromium and molybdenum microcarbides reinforcing the microstructure with the same principal as composite materials
- a very efficient work hardening capability in service, coming from a metallurgic effect called TRIP effect (TRansformation Induced by Plasticity).
In addition to its high wear resistance, CREUSABRO® 8000 still maintains a very good aptitude to processing, far much better than that of 500 HB water quenched. CREUSABRO® 8000 offers consequently the best possible optimization of an exceptional wear resistance and a very acceptable workability. Application markets of CREUSABRO® 8000 are : mines, quarries, cement industries, steel making, publics works.
Iron content calculated as remainder.
Information provided by manufacturer.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Modulus of Elasticity
- Charpy Impact, Notched Low Temp
- CTE, linear 20°C
- CTE, linear 100°C
- CTE, linear 250°C
- CTE, linear 500°C
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|