Industeel CREUSABRO® M Wear Resistant Steel
Subcategory: Carbon Steel; High Carbon Steel; Metal
Key Words: AFNOR Z120M12, EURONORM X120Mn12, WERKSTOFF Nbr W1.3401, OTHER STANDARD "HADFIELD", ASTM A128 Grade B2
Material Notes: Description: CREUSABRO® M is a high Manganese, fully austenitic, quench annealed, non magnetic, work-hardening steel with an exceptionally high level of wear resistance when subjected to work-hardening by shock or high impact pressure in service. The main characteristics is a superior wear resistance: Severe wear on the surface has a work-hardening effect on the austenitic structure of this steel. This, when combined with the level of carbon in accordance with the international standards, leads to an increase in hardness from 200BHN (in as delivered plates) up to an in-service hardness of at least 600BHN. This work-hardening capability renews itself through out in-service life. The underlayers not work-hardened maintain an excellent resistance to shock and a very high ductility.
Iron content calculated as remainder.
Information provided by manufacturer.
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|