Industeel SUPERELSO® 500HR Quenched and Tempered High Strength Steel for Wet H2S Service
Subcategory: Carbon Steel; Medium Carbon Steel; Metal
Key Words: EN10028 part 6 P500QL2, ASTM A 533C Cl. 2 (mod.), ASME II Part A SA 533C Cl. 2 (mod.)
Material Notes: Description: Superelso® 500 HR (SE 500 HR, "Hydrogen Resistant") is a 500MPa (72ksi) yield strength quenched and tempered steel adapted for pressure equipment operating under sour service condition. It is designed to meet the requirements of NACE Standard MR0175, with a maximum hardness of 22 HRC in the heat-affected zone (HAZ) after post weld heat treatment (PWHT). SE 500 HR is manufactured via the electric furnace with dephosphorisation, ladle refining and vacuum degassing to provide a reproducible, clean steel. The use of special steelmaking practice imparting high steel cleanliness, along with a carefully adapted chemistry and a uniform structure provides SE500 HR with excellent resistance to wet H2S cracking, including SSC, HIC and SOHIC. The low carbon content of SE500 HR limits the HAZ hardness after welding and also improves weldability. This steel displays excellent toughness, with a low transition temperature (-60°C/-76°F). This steel is particularly suitable for pressure equipment in wet H2S service in the offshore oil and gas industry, where its high strength allows significant weight and cost reductions.
Iron content calculated as remainder. Mechanical properties for 50-150 mm plates.
Information provided by manufacturer.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Yield
- Charpy Impact, Notched Low Temp
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|