Industeel SUPERELSO® 690CR Quenched and Tempered High Strength Steel for Leg Components of Jack-up Rigs
Subcategory: Carbon Steel; Medium Carbon Steel; Metal
Key Words: DNV NVF 690/grade F, ASTM A514-A517, ABS FH 40
Material Notes: Description: Superelso® 690 CR (SE 690 CR) is a 690MPa (100ksi) yield strength quenched and tempered steel adapted for jack-up rig legs of offshore drilling platforms. Superelso® 690 CR is manufactured via the electric furnace with dephosphorisation, ladle refining and vacuum degassing to provide a reproducible, clean and homogenous steel. This material has been specially designed for offshore applications requiring the use of heavy thick plates (up to 250 mm/10") with demanding mechanical properties requirements. The chemical composition of SE 690 CR has been carefully adapted and allows the achievement of high impact values (> 50 J at -60°C) across the thickness while respecting the tensile properties required. The main application of Superelso® 690 CR being the manufacturing of racks and chords, particular attention has been paid on forming, oxycutting and welding properties. The very low carbon content of this material allows cutting and welding under classical conditions, increasing in the way the cost efficiency of manufacturing.
Iron content calculated as remainder. Mechanical properties for plates with thickness < 210 mm.
Information provided by manufacturer.
| Available Properties |
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Charpy Impact, Notched Low Temp
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|