Johnson Matthey Matti-sil 453 Cadmium Free Brazing Alloy
Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Precious Metal; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Matti-sil 453S has the additions of Silicon which promotes flow and helps produce neat smooth fillets. Optimum Joint Gap 0.05 - 0.15 mm. AWS A5.8-92 BAg-36 Equivalent to Engelhard Silvaloy A-45T Equivalent to Handy & Harman Braze 452 Equivalent to J W Harris Safety-Silv 45T Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|