Johnson Matthey Matti-sil 45 Cadmium Free Brazing Alloy
Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Precious Metal; Nonferrous Metal; Solder/Braze Alloy
Material Notes: A medium flowing alloy which is often used for marine and Shipbuilding applications. Optimum Joint Gap 0.075 - 0.2 mm. AWS A5.8-92 BAg-5 BS EN 1044 1999 AG203 Federal Specification QQ-B-564 BAg-5 Equivalent to Engelhard Silvaloy A-45 Equivalent to Handy & Harman Braze 450 Equivalent to J W Harris Safety-Silv 45 Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |