Johnson Matthey Matti-sil 18Si Cadmium Free Brazing Alloy
Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Precious Metal; Nonferrous Metal; Solder/Braze Alloy
Material Notes: Matti-sil 18Si was developed as an economic alternative to the high silver alloys, particularly for steel automotive components where the higher temperature bronze alloys cannot be tolerated. Optimum Joint Gap 0.075 - 0.2 mm. Information provided by Johnson Matthey.