Johnson Matthey Argo-braze 49LM Silver Brazing Alloy for Tungsten Carbide Brazing
Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Precious Metal; Nonferrous Metal; Solder/Braze Alloy
Material Notes: This material is supplied as Trifoil. Trifoil consists of a layer of copper sandwiched by brazing alloy. The copper helps to absorb the stresses caused by the differential expansion rates, under heating, of carbides and most steel backings. Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|