Johnson Matthey Argo-braze 40N Silver Brazing Alloy for Tungsten Carbide Brazing
Subcategory: Silver Alloy; Copper Alloy; Zinc Alloy; Precious Metal; Nonferrous Metal; Solder/Braze Alloy
Material Notes: An economical alloy for brazing tungsten carbides and stainless steels. Optimum Joint Gap 0.1 - 0.25 mm. AWS A5.8-92 BAg-4 Federal Specification QQ-B-564 BAg-4 Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|