Johnson Matthey Matti-phos 15 Alloy for Fluxless Brazing of Copper
Subcategory: Silver Alloy; Copper Alloy; Precious Metal; Nonferrous Metal; Solder/Braze Alloy
Material Notes: This alloy gives ductile joints on copper to copper and is used by electrical assemblies such as motors and contacts. Optimum Joint Gap 0.05 - 0.2 mm. AWS A5.8-92 BCuP-5 BS EN 1044 1999 CP102; Does not conform exactly to the requirements of EN 1044. Federal Specification QQ-B-650 BCuP-5 Equivalent to Engelhard Silvaloy 15 Equivalent to Handy & Harman Sil-Fos 15 Equivalent to J W Harris Stay-Silv 15 Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|