Johnson Matthey Matti-phos 2 Alloy for Fluxless Brazing of Copper

 

Subcategory: Copper Alloy; Nonferrous Metal; Solder/Braze Alloy

Material Notes:
This alloy is less expensive than other Matti-phos alloys. It has good flow and ductility, and has the same uses as Copper-flo.

Optimum Joint Gap 0.05 - 0.2 mm.
AWS A5.8-92 BCuP-6
BS EN 1044 1999 CP105; Does not conform exactly to the requirements of EN 1044.
Federal Specification QQ-B-650 BCuP-6
Equivalent to Engelhard Silvaloy 2
Equivalent to Handy & Harman Sil Fos 2
Equivalent to J W Harris Stay-Silv 2

Information provided by Johnson Matthey.

Available Properties
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。