Johnson Matthey Matti-phos 2 Alloy for Fluxless Brazing of Copper
Subcategory: Copper Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: This alloy is less expensive than other Matti-phos alloys. It has good flow and ductility, and has the same uses as Copper-flo. Optimum Joint Gap 0.05 - 0.2 mm. AWS A5.8-92 BCuP-6 BS EN 1044 1999 CP105; Does not conform exactly to the requirements of EN 1044. Federal Specification QQ-B-650 BCuP-6 Equivalent to Engelhard Silvaloy 2 Equivalent to Handy & Harman Sil Fos 2 Equivalent to J W Harris Stay-Silv 2 Information provided by Johnson Matthey.