Johnson Matthey Copper-flo AWS Alloy for Fluxless Brazing of Copper
Subcategory: Copper Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: The copper-flo alloys are used for manufacture of heat exchanger return bends, refrigeration pipes and hot water cylinders. Optimum Joint Gap 0.75 - 0.2 mm. AWS A5.8-92 BCuP-2 BS EN 1044 1999 CP202; Does not conform exactly to the requirements of EN 1044. Federal Specification QQ-B-650 BCuP-2 Equivalent to Engelhard Silvaloy 0 Equivalent to Handy & Harman Fos-Flo 7 Equivalent to J W Harris Harris O Information provided by Johnson Matthey.