Johnson Matthey JM Tenacity 2 Brazing Flux Powder
Subcategory: Nonferrous Metal; Solder/Braze Alloy
Material Notes: JM Tenacity No 2 flux is highly active with a working range up to 1480°F. It can be used on most metals, except for Aluminum and magnesium, for brazing with silver brazing alloys. JM Tenacity No 2 fluz powder can be used to braze stainless steel provided that brazing temperature is below 1300°F. JM Tenacity No 2 powder is ideal for hot rodding or application as a water-based paste. Flux residues can be removed with hot water after brazing. Residues:Water soluble Information provided by Johnson Matthey.
|
|
|