Johnson Matthey Mattiflux 100 Brazing Flux Paste
Subcategory: Nonferrous Metal; Solder/Braze Alloy
Material Notes: Mattiflux 100 flux paste is a general purpose flux with a good life at temperature and overheat resistance, being active to 1520°F. It is suitable for use with brazing alloys which have a liquidus of up to 1430°F Flux residues can be removed with hot water after brazing. Residues: Water soluble Information provided by Johnson Matthey.
|
|
|