Johnson Matthey Mattiflux 3A Brazing Flux Paste
Subcategory: Nonferrous Metal; Solder/Braze Alloy
Material Notes: A boron modified flux paste designed for use when brazing tungsten carbide, Stainless steels and the refractory metals (except where interfacial/crevice corrosion is possible). Residues: Water soluble Information provided by Johnson Matthey.
|
|
|