Johnson Matthey JM6236 Soft Solder/Flux
Subcategory: Lead Alloy; Tin Alloy; Nonferrous Metal; Solder/Braze Alloy
Material Notes: General information on the Johnson Matthey soft solder and flux product line: A wide range of Tin/Lead solders suitable for a variety of applications is available from Johnson Matthey. Most materials can be offered as solid wires or as flux cored, to suit the required applications. A wide range of Silver containing solders are suitable for applications where higher strength, increased corrosion resistance or electrical conductivity are required. In some markets the use of Lead or Cadmium containing solders is prohibited in potable water systems, this has led to the increase use of the Silver bearing and Copper bearing-Lead free solders. Solders are available as: Sticks wire (solid or flux cored), preforms, ingots, ribbon bars and solderpaste. ASTM Grade Sn 62 BS.EN 29453 Alloy No. 30
Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|