Johnson Matthey JM No2S Soft Solder Flux
Subcategory: Nonferrous Metal; Solder/Braze Alloy
Material Notes: A liquid non-corrosive flux for use on copper and brass. The residues are water soluble and non-corrosive, however it is recommended they are removed to prevent any possibility of contamination after soldering. Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|