Johnson Matthey JM R-Core Soft Solder Flux
Subcategory: Nonferrous Metal; Solder/Braze Alloy
Material Notes: A "rosin" type core generally used for joining copper and brass. Residues are non-corrosive. Information provided by Johnson Matthey.
| Available Properties |
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|