Kaiser Aluminum Alloy 4026 T651 Rod & Bar

 

Subcategory: Aluminum Alloy; Nonferrous Metal; 4000 Series Aluminum Alloy

Close Analogs: Aluminum content is determined by balance.

Material Notes:
This alloy is used when high strength with wear and/or galling resistance is required. It can eliminate hard-coat anodizing in some applications. Typical applications include air compressor pistons and automotive transmission valve parts. It has good machining characteristics, producing small chips and good surface finish.

  1. Ratings A through E are relative ratings in decreasing order of merit, based on exposures to sodium chloride solution by intermittent spraying or immersion. Alloys with A and B ratings can be used in industrial and seacoast atmospheres without protection. Alloys with C, D and E ratings generally should be protected at least on faying surfaces.
  2. Stress-corrosion cracking ratings are based on service experience and laboratory tests of specimens exposed to the 3.5% sodium chloride alternate immersion test.
    A= No known instance of failure in service or in laboratory tests.
    B= No known instance of failure in service; limited failures in laboratory tests of short transverse specimens.
    C= Service failures with sustained tension stress acting in short transverse direction relative to grain structure; limited failures in laboratory tests of long transverse specimens.
    D= Limited service failures with sustained longitudinal or long transverse
  3. Ratings A through D for Workability (cold), A through E for Machinability and A through C for Anodize Response, are relative ratings in decreasing order of merit.

    Available Properties
    • Hardness, Rockwell B
    • Tensile Strength, Ultimate
    • Tensile Strength, Yield
    • Elongation at Break
    • Modulus of Elasticity
    • Cold Workability3
    • Gall Resistance3
    • General Corrosion Resistance1
    • Machinability3
    • Wear Resistance3
      
    Property Data

    This page displays only the text
    of a material data sheet.

    To see MatWeb's complete data
    sheet for this material (including
    material property data, metal
    compositions, material suppliers,
    etc
    ), please click the button below.

    <meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。