Kinetics MIM 17-4PH Stainless Steel (H900 Condition)

 

Subcategory: Stainless Steel; Precipitation Hardening Stainless; Metal

Close Analogs:

Iron content calculated by difference.

Key Words: Metal Injection Molding, UNS S17400, 17/4PH, 17-4 PH

Material Notes:
Precipitation-hardening stainless steel. Offers a good balance between corrosion resistance and strength. Magnetic. Hardenable to various strength levels and hardness by varying the aging heat treat temperature. Typically provides better corrosion resistance than the 400 series stainless steels, and better strength than the 300 series stainless steels. Often used for aircraft, dental, marine, medical, surgical, and applications where high levels of strength and hardness, and good corrosion resistance is required.

Property values reported are typical for Kinetics' MIM products.

Metal Injection Molding General Notes: Fine metal powders (generally <25 microns in diameter) are combined with a polymer binder system to form a feedstock suitable for injection molding. Kinetics' feedstock is compounded using specific binder and metal powder formulations to control consistency, quality, and dimensional repeatability of parts produced. While standard plastic injection molding machines and molds are used to produce MIM parts, due to the presence of the polymer binder in MIM feedstocks, mold cavities are designed approximately 20% larger than the final part size. Like plastics, MIM molds may have multiple cavities, inserts, slides, unscrewing cores, and hot runner systems. After molding, green parts are debound and sintered at temperatures up to 2,600°F. During debinding, the polymer binder breaks down and dissipates while the metal particles retain all of the molded features. The metal particles fuse together during sintering and the part shrinks approximately 20% to form a solid metal part.

Information provided by Kinetics, Inc.

Available Properties
  • Density
  • Hardness, Rockwell C
  • Ultimate Tensile Strength
  • Tensile Yield Strength
  • Elongation at Break
  • Reduction of Area
  • Surface Finish
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。