Kinetics MIM 440C Stainless Steel
Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal
Close Analogs: Iron content calculated by difference.
Key Words: Metal Injection Molding; UNS S44004
Material Notes: Martensitic stainless steel. Excellent strength, hardness, and wear resistance while offering some corrosion resistance. Magnetic. Often used for automotive, cutlery, industrial equipment, power hand tools, pumps, sporting equipment industry, surgical instruments, valves, and applications where very high strength, hardness, and wear resistance, and some corrosion resistance is required. Property values reported are typical for Kinetics' MIM products. Metal Injection Molding General Notes: Fine metal powders (generally <25 microns in diameter) are combined with a polymer binder system to form a feedstock suitable for injection molding. Kinetics' feedstock is compounded using specific binder and metal powder formulations to control consistency, quality, and dimensional repeatability of parts produced. While standard plastic injection molding machines and molds are used to produce MIM parts, due to the presence of the polymer binder in MIM feedstocks, mold cavities are designed approximately 20% larger than the final part size. Like plastics, MIM molds may have multiple cavities, inserts, slides, unscrewing cores, and hot runner systems. After molding, green parts are debound and sintered at temperatures up to 2,600°F. During debinding, the polymer binder breaks down and dissipates while the metal particles retain all of the molded features. The metal particles fuse together during sintering and the part shrinks approximately 20% to form a solid metal part. Information provided by Kinetics, Inc.
| Available Properties |
- Density
- Ultimate Tensile Strength
- Tensile Yield Strength
- Elongation at Break
- Hardess Rockwell R15N
- Surface Finish
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|