Kobe Steel KSG12 Titanium alloy with low alloying elements, ASTM Gr. 12, Annealed
Subcategory: Titanium Alloy
Close Analogs: Composition Notes: Titanium content calculated as remainder
Material Notes: Nominal Composition: Ti-0.3 Mo-0.8 Ni Applications: Condenser tubes, heat transfer tubes, piping, linings, electrolysis vessels, chemical use. Features: Super corrosion resistant. Information provided by Kobe Steel
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Bend Radius, Minimum
|
|
|
|