Kobe Steel KS15-3-3-3 Beta Titanium Alloy, AMS 4914, Solution treated
Subcategory: Titanium Alloy
Close Analogs: Composition Notes: Titanium content calculated as remainder
Material Notes: Nominal Composition: Ti-15 V-3 Cr-3 Sn-3 AlApplications: Aircraft parts, bicycle gears, gold club heads, foils. Features:Cold workable. Information provided by Kobe Steel
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Bend Radius, Minimum
|
|
|
|