Allegheny Ludlum Duplex Stainless Steel AL 2003™
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Duplex
Key Words: UNS S32003 Composition Notes: Iron content calculated as remainder
Material Notes:
Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride stress corrosion cracking resistance. Applications: DesalinationBridge Decking Oil and GasHome AppliancesHeat Exchangers Pressure Vessels Pulp and Paper Tanks Architectural Structures Water Heaters Power Generation Reinforcing Bar Chemical Processing Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Modulus of Elasticity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|