Allegheny Ludlum Corrosion Resistant Stainless Steel AL 4565™
Subcategory: Stainless Steel; T S30000 Series Stainless Steel; Metal; Austenitic
Key Words: UNS S34565, EN 1.4565 Composition Notes: Iron content calculated as remainder
Material Notes:
Characteristics: Very high resistance to pitting and crevice corrosion Excellent general corrosion resistance in a variety of media Higher mechanical propertied then conventional stainless steels Good weldablility and metallurgical stability Good resistance to stress corrosion crackingInformation provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Modulus of Elasticity
- Volume Resistivity
- CTE, linear 20°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Thermal Conductivity at Elevated Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|