Allegheny Ludlum Dual Stabilized- Low Titanium Stainless Steel AL 468™
Subcategory: Stainless Steel; T S40000 Series Stainless Steel; Metal; Ferritic
Key Words: UNS S46800, ASTM A240 Composition Notes: Iron content calculated as remainder
Material Notes:
Characteristics:good corrosion resistance in a wide range of environments, can be used in annealed cold formed or as-welded conditions. Applications: used in place of Type 304 in an oxidizing when resistance to stress corrosion cracking is needed, use in place of Type 409 at high temperatures, automotive exhaust system components, residential furnace heat exchangers, shell and tube heat exchangers, nuclear applications. Information provided by Allegheny Ludlum
| Available Properties |
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- CTE, linear 20°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Corrosion Rate mils per year
- Corrosion Rate mils per year (base metal)
- Corrosion Rate mils per year (weld)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|