Allegheny Ludlum Nickel-Based, Corrosion Resistant Alloy Allcorr®
Subcategory: Nickel Base
Key Words: UNS N06110 Composition Notes: Iron content calculated as remainder
Material Notes:
Characteristics: non-age hardenable; outstanding resistance to general corrosion, pitting corrosion, crevice corrosion, intergranular corrosion, and stress corrosion cracking; high strength; high ductility, good weldability; good hot and cold workability; good machinability Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Elongation at Break at Elevated Temperature
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|