Allegheny Ludlum Relay Steels No. 2
Key Words: Composition Notes: Iron content calculated as remainder
Material Notes: Silicon and iron alloy Applications:relays, armatures, solenoids, magnetic clutches, pole pieces, certain types of motors, transformers, data processing equipment. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Specific Gravity
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Electrical Resistivity
- Magnetic Coercive Force, Hc
- Magnetic Saturation Flux Density, Bmax
- Magnetic Remanence, Br
- Curie Temperature
|
|
|
|