Allegheny Ludlum Stainless Steel Chromium-Nickel-Manganese AL 201LN™, M-7 (UNS S20153)

 

Subcategory: Stainless Steel; T S20000 Series Stainless Steel; Metal

Material Notes:
Iron content above calculated as balance.

AL 201LN™ is a special composition of Type 201 specifically for sub-zero temperature service as welded tanks and vessels. This alloy has replaced the familiar 300 series stainlesses such as type 301 or type 304 in many applications based upon technical equivalency and economic considerations. AL 201LN alloy is a natural choice for use at temperatures down to -320°F. The alloy is suited for many ambient temperature structural applications, such as railroad freight cars, truck trailers, coal handling and other bulk transport equipment where there is need for a good combination of corrosion resistance, strength, toughness and ease of fabrication.

Information provided by Allegheny Ludlum Corporation.

Available Properties
  • Density
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break at Elevated Temperature
  • Izod Impact
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。