Allegheny Ludlum AL 2205™ Duplex Stainless Steel, Sheet and Strip < 0.1875", UNS S31803
Subcategory: Stainless Steel; Metal
Key Words: DIN 1.4462; ASTM A-240; ASME SA-240
Material Notes: Iron content above calculated as remainder. Ferromagnetic. The AL 2205 alloy is a nitrogen-enhanced duplex stainless steel alloy. The nitrogen serves to significantly improved the corrosion resistance of the alloy; especially in the welded condition. Earlier duplex alloys have had moderate resistance to general corrosion and chloride stress corrosion cracking, but suffered a substantial loss of properties when used in the as-welded condition. To impart the metallurgical benefits of nitrogen to both improved corrosion performance and as-welded properties, the AL 2205 alloy is produced to a .15% minimum nitrogen content compared to the ASTM range of .08-.20%. The minimum Cr, Mo, and Ni contents of AL 2205 alloy are all above the mid range of the ASTM composition specification. When heat-treated properly, the nominal 22% chromium, 5.5% nickel, 3% molybdenum, and 0.16% nitrogen in the AL 2205 alloy produces a microstructure that consists of nearly equal mixture of austenite and ferrite phases. The microstructure and composition of the AL 2205 alloy provides corrosion resistance to many environments that is superior to Types 316, and a yield strength that is more than double that of conventional austenitic stainless steels. The microstructure and phase balance of AL 2205 alloy have been designed to facilitate the production of pipe and tube products. All AL 2205 alloy is metallographically examined to ensure that the as-shipped product is essentially free from the presence of detrimental precipitate phases such as sigma. The AL 2205 is the most widely used of the duplex stainless steels and is often used in the form of welded pipe or tubular components. The alloy has also been applied as a formed and welded sheet product in environments where resistance to general corrosion and chloride stress corrosion cracking is important. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Rockwell C
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- CTE, linear 20°C
- Specific Heat Capacity
- Thermal Conductivity
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|