Allegheny Ludlum AL 29-4C® Stainless Steel, UNS S44735
Subcategory: Stainless Steel; Metal
Key Words: ASTM A-240
Material Notes: Iron content above calculated as remainder; Nb content above includes Ti. AL 29-4C alloy is a superferritic stainless steel designed by Allegheny Ludlum for extreme resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking, as well as general corrosion in oxidizing and moderately reducing environments. The alloy was developed in the early 1980s for welded condenser tubing to be used in seawater and brackish water by the power generation industry. It is this extreme resistance to pitting and crevice corrosion that has led to the installation of over 2000 miles of AL-29-4C tubing in power plant condensers and heat exchangers. The superferritic stainless steel AL 29-4C alloy shows excellent resistance to chloride ion pitting, crevice corrosion and stress corrosion cracking. This resistance makes it an ideal choice for battling the corrosive condensate of partially and fully condensing natural gas and propane burning appliances. Its low alloy content, compared to other high-performance alloys, makes it an economical choice as well. Property data below is typical of annealed samples. Information provided by Allegheny Ludlum.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|