Allegheny Ludlum Type 316 Stainless Steel, UNS S31600

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal

Material Notes:
Iron content above calculated as remainder.

This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels such as Type 304. These alloys also offer higher creep, stress-to-rupture and tensile strength at elevated temperature. Types 317 and 317L containing 3 to 4% molybdenum are preferred to Types 316 or 316L which contain 2 to 3% molybdenum in applications requiring enhanced pitting and general corrosion resistance. Austenitic stainless steels with higher molybdenum or molybdenum plus nitrogen content which provide even greater resistance to pitting, crevice corrosion an general corrosion are also available in flat-rolled products from Allegheny Ludlum. Properties of these alloys are described in separate technical data publications available from Allegheny Ludlum. In addition to excellent corrosion resistance and strength properties, this alloy also provides the excellent fabricability and formability. This is available in the form of sheet, strip and plate to ASTM A240 and ASME SA-240 and other pertinent specifications.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Hardness, Brinell
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Modulus of Elasticity
  • Charpy Impact
  • Shear Modulus
  • Electrical Resistivity
  • CTE, linear 20°C
  • CTE, linear 500°C
  • CTE, linear 1000°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  • Maximum Service Temperature, Air
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。