Allegheny Ludlum Type 317 Stainless Steel, UNS S31700
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Material Notes: Iron content above calculated as remainder. This is a molybdenum-bearing austenitic stainless steels which is more resistant to general corrosion and pitting/crevice corrosion than the conventional chromium-nickel austenitic stainless steels such as Type 304. These alloys also offer higher creep, stress-to-rupture and tensile strength at elevated temperature. Types 317 and 317L containing 3 to 4% molybdenum are preferred to Types 316 or 316L which contain 2 to 3% molybdenum in applications requiring enhanced pitting and general corrosion resistance. Austenitic stainless steels with higher molybdenum or molybdenum plus nitrogen content which provide even greater resistance to pitting, crevice corrosion an general corrosion are also available in flat-rolled products from Allegheny Ludlum. Properties of these alloys are described in separate technical data publications available from Allegheny Ludlum. In addition to excellent corrosion resistance and strength properties, this alloy also provides the excellent fabricability and formability. This is available in the form of sheet, strip and plate to ASTM A240 and ASME SA-240 and other pertinent specifications. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Brinell
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Shear Modulus
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|