Allegheny Ludlum Stainless Steel Chromium-Nickel-Molybdenum 317L (UNS S31703)
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: Plate, sheet, and tube spec is ASTM A-240
Material Notes: Iron content above calculated as balance. Allegheny Ludlum's 317L™ is molybdenum-bearing austenitic stainless steel with greatly increased resistance to chemical attack as compared to the conventional chromium-nickel austenitic stainless steels such as Type 304. AL 317L™ alloy also offers higher creep, stress-to-rupture, and tensile strength at elevated temperatures than conventional stainless steels. The alloy has low carbon to provide resistance to sensitization during welding and other thermal processes. This alloy is intended for severe service conditions such as flue gas desulfurization (FGD) systems. Information provided by Allegheny Ludlum Corporation.
| Available Properties |
- Density
- Hardness, Brinell
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- Magnetic Permeability
- CTE, linear 20°C
- CTE, linear 500°C
- CTE, linear 1000°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|