Allegheny Ludlum Type 332 Stainless Steel, UNS N08800

 

Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal

Material Notes:
Iron content above calculated as remainder.

Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both to chloride stress corrosion cracking and to embrittlement from precipitation to sigma phase. The general corrosion resistance is excellent. In the solution annealed condition, Type 332 has superior creep and stress rupture properties. Type 332 has been approved as a material of construction under ASME Boiler and Pressure Vessel Code, Section I - Power Boilers, Section III - Nuclear Vessels, Section VIII - Unfired Pressure Vessels.

Information provided by Allegheny Ludlum

Available Properties
  • Density
  • Tensile Strength, Ultimate
  • Tensile Strength, Yield
  • Elongation at Break
  • Reduction of Area
  • Electrical Resistivity
  • Magnetic Permeability
  • Curie Temperature
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  • Melting Point
  • Solidus
  • Liquidus
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。