Allegheny Ludlum Type 332 Stainless Steel, UNS N08800
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Material Notes: Iron content above calculated as remainder. Type 332 is a nickel and chromium austenitic stainless steel designed to resist oxidation and carburization at elevated temperatures. The nickel content, 32%, makes the alloy highly resistant both to chloride stress corrosion cracking and to embrittlement from precipitation to sigma phase. The general corrosion resistance is excellent. In the solution annealed condition, Type 332 has superior creep and stress rupture properties. Type 332 has been approved as a material of construction under ASME Boiler and Pressure Vessel Code, Section I - Power Boilers, Section III - Nuclear Vessels, Section VIII - Unfired Pressure Vessels. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
- Reduction of Area
- Electrical Resistivity
- Magnetic Permeability
- Curie Temperature
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Specific Heat Capacity
- Thermal Conductivity
- Melting Point
- Solidus
- Liquidus
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|