Allegheny Ludlum Stainless Steel 334 (UNS S33400)
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Material Notes: Iron content above calculated as balance. Allegheny Ludlum Type 334 is a titanium- and aluminum-bearing austenitic stainless steel offering superior elevated temperature scaling resistance compared to the conventional chromium-nickel stainless steels such as Type 304. The oxidation resistance of Type 334 compares favorably with higher alloyed grades up to 1900°F, making it a good candidate alloy for use in emission control systems, and other applications where resistance to elevated temperature degradation is important. Information provided by Allegheny Ludlum Corporation.
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Ultimate at Elevated Temperature
- Tensile Strength, Yield
- Tensile Strength, Yield at Elevated Temperature
- Elongation at Break
- Modulus of Elasticity
- Electrical Resistivity
- CTE, linear 20°C
- CTE, linear 250°C
- CTE, linear 500°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|