Allegheny Ludlum AM 350™ High Strength Specialty Steel Alloy, UNS S35000
Subcategory: Stainless Steel; T 300 Series Stainless Steel; Metal
Key Words: ASTM A-693; ASME SA-693; AMS 5548
Material Notes: Iron content above calculated as remainder. Property data below is typical of annealed samples. Available in sheet and strip only. For use in valves, aircraft tubing, bellows, mounts, brackets, and ducts. Information provided by Allegheny Ludlum
| Available Properties |
- Density
- Hardness, Rockwell B
- Tensile Strength, Ultimate
- Tensile Strength, Yield
- Elongation at Break
|
|
|
|