MatWeb - Material Property Data 用 MatWeb 登广告!    Register Now
越过59,000 以上, 金属、塑料、陶瓷和合成物的数据资料库。
MatWeb - Material Property Data 主页  •  搜寻  •  工具  •  供应商  •  文件夹  •  有关我们  •  常用问题  •  登录   •  English English English 
  搜寻方法:  高级先进 | 材料类型 | 特性 | 构成份  | 商标  | 制造商
    Search

Subscribe to FREE Trade Publications!

Allegheny Ludlum AL 433™ Ferritic Stainless Steel, Annealed

 

Subcategory: T 400 Series Stainless Steel; Stainless Steel; Metal

Material Notes:
Iron content above calculated as balance.

AL 433™ is a stainless steel in the ferritic family of alloys with Type 409 and Type 439. The AL 433 alloy contains 20% chromium for pitting and crevice corrosion resistancein the presence of chlorides and resistance to oxidation at elevated temperatures. An addition of 0.5% copper adds to corrosion resistance. Columbium (niobium) in the amount of about 0.5% is added for elevated temperature strength and also provides resistance to intergranular corrosion.

The AL 433 alloy has a body-centered cubic, ferritic microstructure at all temperatures below the melting point. Fine columbium carbides may be visible in the ferrite matrix microstructure.

The AL 433 alloy can be machined, welded and formed like other stabilized, ferritic stainless steels. AL 433 alloy is an excellent candidate for elevated temperature applications where strength, combined with fabricability are needed.

Information provided by Allegheny Ludlum Corporation.

Available Properties
  • Density
  • Hardness, Rockwell B
  • Tensile Strength, Ultimate
  • Tensile Strength, Ultimate at Elevated Temperature
  • Tensile Strength, Yield
  • Tensile Strength, Yield at Elevated Temperature
  • Elongation at Break
  • Modulus of Elasticity
  • CTE, linear 20°C
  • CTE, linear 250°C
  • CTE, linear 500°C
  • Specific Heat Capacity
  • Thermal Conductivity
  
Property Data

This page displays only the text
of a material data sheet.

To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc
), please click the button below.

<meta http-equiv=Content-Type content="text/html; charset=UTF-8">
请读关于材料数据的使用许可协议和我们的隐私权。询问或评论有关 MatWeb? 请与webmaster@matweb.com 联系。我们感谢您对 MatWeb的参与。

本站点由 Automation Creations, Inc. 设计和维护。这个网站的内容, MatWeb 的商标,与 "MatWeb" 由 Automation Creations, Inc.版权1996-2006拥有 。 MatWeb 意欲为个人使用 , 非商业用途。这个站点的内容、结果和技术数据,未经由 Automation Creations, Inc. 允许, 不可以被电子,摄影或实质上地再生产或自动化创作。