Allegheny Ludlum AL 50™ High Strength Stainless Steel, UNS S20910
Subcategory: Stainless Steel; Metal
Material Notes: Iron content above calculated as remainder. Nitrogen-strengthened austenitic stainless steel for petrochemical, pulp and paper and food processing industries. Available in plate form. Information provided by Allegheny Ludlum
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |